fiber laser cell scribing machine cell cutting machine solar panel making machines and manufacturing machines

Type:

Specification:

Profile:

 Fiber  laser solar cell cutting machine

  

Model: OLS-20F





Solar Cell Laser Scribing Machine Function


scribing or cutting the Solar Cells and Silicon Wafers in solar PV industry, including the mono-si (mono crystalline silicon) and poly-si (poly crystalline silicon) solar cells and silicon wafer. 

 

Fiber Solar Cell Laser Cutting Machine Features


1. Using the Germany IPG FIBER laser or China Raycus Fiber laser or Max fiber laser

  service time over  100,000hours.

 Stronger adaptability to enviroment

  better beam quality and higher speed than Diode Pump and YAG Krypton type.

 No need to replace the laser module and Krypton lamp.

 

2. Work table: X-Y movable

  Solar cell can be automatic absoption

 

3.Air cooling, compact structure, small size

 

4. higher conversion efficency, lower operating cost, save power consumption

 cost and shorter maintenance time;

 

5. Laser Pulse width is more narrow, Higher peak power, faster scribing cutting speed

6.Long time uninterrupted continuous maintenance-free operation, no consumable wearing parts to replace

7. Stepper motor or servo motor different cost.


Fiber Laser Scribing Machine Technical Parameters



Model

OLS-10F OLS-20F

Laser wavelength

1064nm

Laser power

10W/20W

Scribing width

30μm

Scribing speed

160mm/s  200mm/s

Scribing accuracy

±10μm

Working area

350x350mm (13.8in*13.8in)

Temperature control precision

0.5°C

Working power

220V/50Hz/1kvA

Working table

negative pressure absorbing and dust elimination

Cooling method

Forced air cooling


Fiber Laser Scribing Machine Main Parts



Diode Solar Cell Laser Scribing Machine Features



1. Using the Diode Side Pump or Semiconductor side pump laser

    service time over  12,000hours.

     better beam quality and higher speed than YAG Krypton type.

     No need to replace the Krypton lamp

2. Import UK acousto optic modulator, high qualiy

3. Work table: X-Y movable

             Solar cell can be automatic absoption, no need to use foot pedal

             350*350mm size

4.Unified constant water chiller: stable and reliable for long period running

 

5. higher integration, better beam quality and higher speed, but lower processing

 cost and shorter maintenance time;

 

6.  no exterior connect

7.  Easy to instal and move the equipment;

8. Improved and new generation machine, Updated 5.0 software;


Diode Solar Cell Laser Cutting Machine Technical Parameters


Model

OLS-50D

Laser wavelength

1064nm

Laser power

50W

Scribing width 

50μm

Scribing speed

120mm/s

Scribing accuracy

±10μm

Click: 2475 Update: 2018-07-12 15:05:26【Print】【Back

What can we do for you

We will reply within 2 hours


Get More Information,
Please Email To:
Sales:
Technical:
Aftersales:

Send to us We will reply within 2 hours, and all information will be safety saved by SSL.
  • skype:margret200789
  • Call us
  • Send SMS